"Reducing distortion and fatigue in metal components"
Less Scrap and Rework
Meta-Lax Weld Conditioning Benefit #5
“Normal welding resulted in
3-inch distortion in 50-feet. We had to scrap the wing checking fixture. When we added Meta-Lax during welding we held distortion to 1/4-inch."
J&J Burning
Bonal Technologies, Inc.